Summertime Printing

It’s summer, but BadDevices never goes to holiday; we are trying to obtain the best from our BadPrinters by printing some big and nice object and we are also concentrating in tweaking the correct parameters for dual printing.

Here some of our latest pieces

DSC_6243 DSC_6249 DSC_6251 DSC_6252 DSC_6253 DSC_6254 DSC_6258

And some work in progress, like the awesome multi-part GE jet engine (the main fan is missing in the picture) and some “mistery” object 🙂

DSC_6262
DSC_6265

Learning Kisslicer

After long time finally our business cards are arrived…
Now we are ready 😀 😀

Image

 

We are dealing with Kisslicer and discovering its features.
In the image you can see the printing difference between a layer 0,1mm on the left, and 0,2mm on the right.

Image

 

But there is more…
I was printing at 0,1 a yellow washer for my intuos pen, but it come out not perfect,
so i try with a different parameter (width extrusion at 0,2) and i was surprised again.
You can see the difference; on the left the “bugged” one, on the right the one printed with a thinner width.

Image

 

🙂